A farm run on the soft card: dry TPU 85A first — that step is not written on the 95A card

Two unlabeled spools apart on a packing table, one matte charcoal and one pale blue

A farm run on the soft card dries TPU 85A first. That step is written on the 85A card. It is not written on the 95A card. We sell FOB Foshan. The factory is in Foshan, Guangdong, next to Guangzhou.

The numbers are the catalog. TPU 85A: impact 120 kJ/m², print 210–240°C, bed 40–60°C, 1.75 mm, ±0.03 mm, three colors — black, transparent and grey. The card says it is softer than 95A, for phone cases, dampers, soft-touch parts and cushioning, and it says dry well before farm runs. TPU 95A: impact 120 kJ/m², print 210–240°C, bed 40–60°C, 1.75 mm, ±0.03 mm, about eight colors including clear tints. The card says it is firmer than 85A, for seals, wheels, grips and protective covers. It does not say dry well before farm runs. The print window matches. The impact number matches. Putting the dry-before-farm sentence on a 95A line is not what that card says.

The Shore name still chooses the line. A phone case, damper or cushion stays on 85A, and that farm run follows the dry sentence on that card. A seal, wheel, grip or cover asked as 95A stays on 95A. A middle gasket stays on 90A: that card names black, white, grey, red, blue, yellow, green and transparent, and it also does not write dry well before farm runs. Each card is 1–2 sample rolls, then its own 50 kg. The cards do not share one 50 kg. 7 filament lines, 400 kg a day on one line and 2.8 tons a day when all 7 run, with in-house material development and color masterbatch, in Foshan next to Guangzhou, is the capacity behind either line. Ocean freight stays on the buyer’s forwarder. FOB Foshan. This note does not add a dryer setpoint, a drying time, or a medical or dental use. The card says dry well. It does not print hours or degrees for that step.

Order check: the farm run is phone cases, dampers or cushioning → TPU 85A, dry the spool before that farm run, then 50 kg. The line is seals, wheels, grips or covers on the firmer card → TPU 95A, without copying the 85A drying sentence onto that card. Both cards → two lines.

Email for a quote: evans@qs3dprinterfilament.com · WhatsApp +852 5307 0568.

Two strands. The softer grey is TPU 85A. The clearer tint is TPU 95A. FOB Foshan.

Which card the farm run takes

TPU 85ATPU 95A
WhenFarm run of phone cases, dampers, cushioningSeals, wheels, grips, covers
Shore85A, softer95A, firmer
Impact120 kJ/m²120 kJ/m²
Print / bed210–240°C / 40–60°C210–240°C / 40–60°C
Diameter1.75 mm · ±0.03 mm1.75 mm · ±0.03 mm
Colors3: black, transparent, greyAbout 8, including clear tints
Farm noteDry well before farm runsThat sentence is not on this card
The 50 kgIts own line after 1–2 sample rollsIts own line after 1–2 sample rolls
The open dryer is the farm step written on the 85A card. The sealed spool is the 95A card, which does not write that step. FOB Foshan.

Grades: TPU 85A · TPU 95A. Compare: TPU 85A vs 95A · cushion stays on 85A.

Factory in Foshan, next to Guangzhou. 7 filament lines, 400 kg a day on one line and 2.8 tons a day when all 7 run, with in-house material development and color masterbatch. Samples 1–2 rolls, then 50 kg on the card the line names. FOB Foshan. evans@qs3dprinterfilament.com · WhatsApp +852 5307 0568.

← Back to articles